This diagram provides an overview of Testex Tape procedures and background information which may improve your Testex Tape results.
This diagram provides an overview of Testex Tape procedures and background information which may improve your Testex Tape results.
The Elcometer 124 Thickness Gauge is used to measure the peak-to-valley height of a surface profile molded from Elcometer 122 Testex Replica Tape. Available in both Metric and Imperial versions. Quick and easy to use. Anvil pressure as required.
Elcometer 122 Testex Replica Tape consists of foam with a non-compressible backing. The foam side is rubbed into the surface providing a permanent mold of the peak-to-valley profile, which can then be measured using the Elcometer 124 Thickness Gauge. Elcometer 122 Testex Tape is available in three profile ranges: Coarse, X-Coarse, and X-Coarse Plus. It [...]
This diagram provides an overview of Testex Tape procedures and background information which may improve your Testex Tape results.
To preview a photo gallery of our other products/product lines, please visit us at www.paintteststore.com. Elcometer University is also “At Your Service” for product tutorials and FAQs at www.elcometeruniversity.com.
The Elcometer 124 Thickness Gauge is used to measure the peak-to-valley height of a surface profile molded from Elcometer 122 Testex Replica Tape.
Elcometer 122 Testex Replica Tape consists of foam with a non-compressible backing. The foam side is rubbed into the surface providing a permanent mold of the peak-to-valley profile, which can then be measured using the Elcometer 124 Thickness Gauge.
Elcometer 122 Testex Tape is available in three profile ranges: Coarse, X-Coarse, and X-Coarse Plus. It is important that the tape grade chosen is reflective of the profile being measured, as using tape grade below the actual value may provide a “false” reading.